Abstract
Ni release from Danish 1 krone coins and metal buttons from jeans was measured at 20.degree. C in distilled water and at 35.degree. C in distilled water and synthetic sweat. The temperature elevation increased the Ni release from the coins and 2 of the 9 metal buttons investigated. The sensitivity to temperature elevation differs from 1 alloy to another. [These results were discussed in light of Ni induced contact sensitization
Original language | English |
---|---|
Journal | Contact Dermatitis |
Volume | 5 |
Issue number | 2 |
Pages (from-to) | 82-84 |
ISSN | 0105-1873 |
DOIs | |