Rh-MnO Interface Sites Formed by Atomic Layer Deposition Promote Syngas Conversion to Higher Oxygenates

Nuoya Yang, Jong Suk Yoo, Julia Schumann, Pallavi Bothra, Joseph A. Singh, Eduardo Valle, Frank Abild-Pedersen, Jens K. Nørskov, Stacey F. Bent*

*Corresponding author for this work

Research output: Contribution to journalJournal articleResearchpeer-review

Abstract

Rhodium (Rh) catalysts are among the major candidates for syngas conversion to higher oxygenates (C2+oxy), with manganese (Mn) as a commonly used promoter for enhancing the activity and selectivity toward C2+oxy. In this study, we use atomic layer deposition (ALD) to controllably modify Rh catalysts with MnO, by depositing manganese oxide as a support layer or an overlayer, in order to identify the function of the Mn promoter. We also compare the ALD-modified catalysts with those prepared by coimpregnation. An ultrathin MnO support layer shows the most effective enhancement for C2+oxy production. Transmission electron microscopy, temperature-programmed reduction, and diffuse reflectance infrared Fourier transform spectroscopy characterization indicates that formation of Rh-MnO interface sites is responsible for the observed activity and selectivity improvements, while ruling out Rh nanoparticle size and alloy or mixed oxide formation as significant contributors. MnO overlayers on Rh appear to suffer from poor stability upon CO adsorption and are less effective than a MnO support layer. Density functional theory (DFT) calculations show that MnO species on the Rh(111) surface lower the transition state energy for CO bond dissociation and stabilize the key transition state for C2+oxy synthesis more significantly than that for methane synthesis, leading to enhanced activity and C2+oxy selectivity.

Original languageEnglish
JournalACS Catalysis
Volume7
Issue number9
Pages (from-to)5746-5757
Number of pages12
ISSN2155-5435
DOIs
Publication statusPublished - 2017
Externally publishedYes

Keywords

  • Atomic layer deposition
  • Catalytic promoter
  • Higher oxygenates synthesis
  • Rh catalyst
  • Syngas conversion

Fingerprint Dive into the research topics of 'Rh-MnO Interface Sites Formed by Atomic Layer Deposition Promote Syngas Conversion to Higher Oxygenates'. Together they form a unique fingerprint.