Pitting Corrosion Behaviour of Boron Added Modified 9Cr-1Mo Steel: Combined Effects of Alkali and Chloride Ions

  • Namrata Upadhyay
  • , M. G. Pujar
  • , C. R. Das
  • , Nanda Gopal Krishna
  • , C. Mallika
  • , U. Kamachi Mudali
  • Indira Gandhi Centre for Atomic Research

Research output: Contribution to journal › Journal article › Research › peer-review

1 Downloads (Orbit)

Abstract

Pitting corrosion behaviour of modified 9Cr-1Mo ferritic steel containing 100 ppm of boron was studied in deaerated 0.1, 0.2 and 0.5 M sodium hydroxide solutions containing 0.1, 0.2 and 0.5 M sodium chloride. The chemical compositions of the passive film developed at applied potentials were studied using XPS. E-pit values decreased with increase in chloride concentrations for the given concentration of alkali. The effect (of Cl-) was less pronounced in higher alkali concentrations. Pit diameters were observed to be significantly higher in 0.1 M sodium hydroxide containing 0.1 M sodium chloride; with increase in alkali concentration pit diameters were found to be restricted to lower values even at higher chloride concentrations. Energy dispersive spectroscopic (EDS) studies showed that pits had nucleated at Al2O3 inclusions/matrix interface. XPS analysis revealed the presence of Fe3O4, Fe(OH)(3) at lower potentials (150 and 209 mV(SCE)) whereas Fe2O3, Fe(OH)(3) and FeO2 (2-) at higher potentials (400 and 650 mV(SCE)).
Original languageEnglish
JournalTransactions of the Indian Institute of Metals
Volume68
Issue number1
Pages (from-to)129-141
ISSN0972-2815
DOIs
Publication statusPublished - 2015
Externally publishedYes

Keywords

  • 9Cr–1Mo steel
  • Alkali
  • Chloride
  • Passive film
  • Pitting corrosion
  • XPS analysis

Fingerprint

Dive into the research topics of 'Pitting Corrosion Behaviour of Boron Added Modified 9Cr-1Mo Steel: Combined Effects of Alkali and Chloride Ions'. Together they form a unique fingerprint.

Cite this