Abstract
A new double vacuum melting route (conventional second refining + vacuum
arc refining [CSR + VAR]) with 33% lower production cost than the
traditional VIM + VAR route has been tried. Compared with the CSR route,
the CSR + VAR route reduces the average inclusion size from
27.1 ± 12.3 μm to 13.7 ± 2.4 μm, and the CSR + VAR steel processes a
13.1% higher rotatory bending fatigue (RBF) fatigue strength (
𝜎−1) and a 3-timeslonger RCF L10
life. The crescent-shaped granular bright facet (GBF) zone, normally
found in high-strength steels' very high cycle fatigue regimes beyond 107 cycles
normally under a much lower stress amplitude, appears around inner
inclusions on the CSR + VAR steel RBF fracture surfaces in high cycle
fatigue regimes beyond 3 × 105 cycles. The development of GBF
zones is estimated to account for 79%–90% of the RBF fatigue life. The
average crack propagation rate (da/dN) for GBF zones varies from
1.3 × 10−12 m/cycle to 24 × 10−12 m/cycle and increases with the stress amplitude.
| Original language | English |
|---|---|
| Journal | Fatigue and Fracture of Engineering Materials and Structures |
| Volume | 45 |
| Issue number | 7 |
| Pages (from-to) | 1995-2009 |
| ISSN | 8756-758X |
| DOIs | |
| Publication status | Published - 2022 |
Keywords
- Crescent-shaped GBF zones
- High carbon bearing steel
- Non-metallic inclusions
- Rolling contact fatigue
- Rotatory bending fatigue
Fingerprint
Dive into the research topics of 'Improve fatigue and mechanical properties of high carbon bearing steel by a new double vacuum melting route'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver