Hot Corrosion Service Testing of Ni-based Superalloys and Correlation with Oxide Scale Calculations

Uffe Bihlet, Kristian Vinter Dahl, Harro A. Hoeg, Marcel A. J. Somers

Research output: Contribution to conferencePosterResearch

365 Downloads (Pure)
Original languageEnglish
Publication date2012
Publication statusPublished - 2012