Abstract
Despite the rapid deployment of bifacial photovoltaic modules, few studies report their degradation outside accelerated stress testing. In this study, we analyze the degradation of 189 PERC modules from four types after 2.1 to 4.5 years of outdoor exposure in the Danish climate. From flash testing, we find a weighted mean Rd of 0.63%/a on the front side compared to datasheet specification, exceeding the 0.5%/a benchmark for monofacial modules. Electroluminescence imaging showed a dark imprint around three sides on the perimeter of half-cut solar cells in one module type. Though rarely described in literature, the fault matches a report about UV-induced degradation. Its impact on Pmp degradation is limited to 0.75%/a in the first 2.5 years. On modules from non-serial production, we observed potential-induced degradation, which caused high current and power loss more prominently on the rear side. On frameless modules, backside glass breakage occurred during operation, primarily caused by rock chipping from mowing activities. Handling also induced breakage when modules were removed from substructures and stacked. In contrast, framed glass-glass modules proved more robust. Additionally, we observed dark cell edges, line cracks, busbar issues, finger contact issues, dark spots, and a hotspot.
| Original language | English |
|---|---|
| Article number | 113786 |
| Journal | Solar Energy |
| Volume | 300 |
| Number of pages | 14 |
| ISSN | 0038-092X |
| DOIs | |
| Publication status | Published - 2025 |
UN SDGs
This output contributes to the following UN Sustainable Development Goals (SDGs)
-
SDG 7 Affordable and Clean Energy
-
SDG 13 Climate Action
Keywords
- Bifacial PV
- Degradation
- Electroluminescence
- Flash test
- I-V-curve
Fingerprint
Dive into the research topics of 'Field degradation of bifacial photovoltaic modules in northern Europe'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver