Experimental studies on hydrogen hydrate with tetrahydrofuran by differential scanning calorimeter and in-situ Raman

Research output: Contribution to journalJournal article – Annual report year: 2019Researchpeer-review

View graph of relations

Clathrate hydrate is a kind of environment-friendly material for storing hydrogen under a certain condition of temperature and pressure. In this work, tetrahydrofuran aqueous solution with concentration of 3.0 mol% was adopted to investigate hydrogen storage process. Moreover, thermal property of hydrate was measured by high pressure differential scanning calorimeter, and mechanism of hydrate-based hydrogen storage was studied by insitu Raman. Especially, gas uptake, morphology and structures change of compounds from gas/liquid interface towards hydrate layer were monitored in the process of hydrate formation. Thermal experiments illustrate that thermal data for tetrahydrofuran-hydrogen binary hydrate under extra high pressures could be effectively obtained by high pressure differential scanning calorimeter, moreover, memory effect shows no influence on thermal state of hydrate but weakly affects water aggregation. Kinetics and microscopic experiments illustrate that a special pressure drop and some tetrahydrofuran hydrates with unstable structure can be found under conditions of 273.15 K and 14.53 MPa. The pressure drop involves into hydrogen molecules tunneling movement among hydrate cavities. Moreover, hydrogen molecules show a positive effect on binary hydrate stability. Further, the density of 1.875 g/Lwater shows that hydrogen storage process via clathrate hydrate is an excellent method to store hydrogen.
Original languageEnglish
JournalApplied Energy
Volume243
Pages (from-to)1-9
ISSN0306-2619
DOIs
Publication statusPublished - 2019
CitationsWeb of Science® Times Cited: No match on DOI

    Research areas

  • Hydrate, Hydrogen storage, Tetrahydrofuran, In-situ Raman

ID: 172638816