The present invention provides a method for sintering, comprising in the following order the steps of: providing a body in the green state or in the pre-sintered state on a support; providing a load on at least one spacer on the support such that the load is located above said body in the green state or in the pre-sintered state without contacting the body; heat treating the body in the green state or in the pre-sintered state at a temperature above the decomposition temperature of organic components contained in the green body and below the softening temperature or decomposition temperature of the spacer; heat treating the body in the green state or in the pre-sintered state at a temperature above the softening point or decomposition temperature of the spacer and below a sintering temperature such that the load contacts the body, and - sintering the body in the green state or pre-sintered state.
Original languageEnglish
IPCC04B35/64
Patent numberWO2012003937
Filing date12/01/2012
CountryDenmark
Publication statusPublished - 2012

Bibliographical note

DTU reference nummer: 92705-11

Cite this

Linderoth, S. (2012). IPC No. C04B35/64. A method for sintering. (Patent No. WO2012003937).
Linderoth, Søren (Inventor). / A method for sintering. IPC No.: C04B35/64. Patent No.: WO2012003937. Jan 12, 2012.
@misc{0d52d6ec889347399ed9ca4d7f5e171a,
title = "A method for sintering",
abstract = "The present invention provides a method for sintering, comprising in the following order the steps of: providing a body in the green state or in the pre-sintered state on a support; providing a load on at least one spacer on the support such that the load is located above said body in the green state or in the pre-sintered state without contacting the body; heat treating the body in the green state or in the pre-sintered state at a temperature above the decomposition temperature of organic components contained in the green body and below the softening temperature or decomposition temperature of the spacer; heat treating the body in the green state or in the pre-sintered state at a temperature above the softening point or decomposition temperature of the spacer and below a sintering temperature such that the load contacts the body, and - sintering the body in the green state or pre-sintered state.",
author = "S{\o}ren Linderoth",
note = "DTU reference nummer: 92705-11; WO2012003937; C04B35/64",
year = "2012",
language = "English",
type = "Patent",

}

Linderoth, S Jan. 12 2012, A method for sintering, Patent No. WO2012003937, IPC No. C04B35/64.

A method for sintering. / Linderoth, Søren (Inventor).

IPC No.: C04B35/64. Patent No.: WO2012003937. Jan 12, 2012.

Research output: Patent

TY - PAT

T1 - A method for sintering

AU - Linderoth, Søren

N1 - DTU reference nummer: 92705-11

PY - 2012

Y1 - 2012

N2 - The present invention provides a method for sintering, comprising in the following order the steps of: providing a body in the green state or in the pre-sintered state on a support; providing a load on at least one spacer on the support such that the load is located above said body in the green state or in the pre-sintered state without contacting the body; heat treating the body in the green state or in the pre-sintered state at a temperature above the decomposition temperature of organic components contained in the green body and below the softening temperature or decomposition temperature of the spacer; heat treating the body in the green state or in the pre-sintered state at a temperature above the softening point or decomposition temperature of the spacer and below a sintering temperature such that the load contacts the body, and - sintering the body in the green state or pre-sintered state.

AB - The present invention provides a method for sintering, comprising in the following order the steps of: providing a body in the green state or in the pre-sintered state on a support; providing a load on at least one spacer on the support such that the load is located above said body in the green state or in the pre-sintered state without contacting the body; heat treating the body in the green state or in the pre-sintered state at a temperature above the decomposition temperature of organic components contained in the green body and below the softening temperature or decomposition temperature of the spacer; heat treating the body in the green state or in the pre-sintered state at a temperature above the softening point or decomposition temperature of the spacer and below a sintering temperature such that the load contacts the body, and - sintering the body in the green state or pre-sintered state.

M3 - Patent

M1 - WO2012003937

Y2 - 2012/01/12

ER -

Linderoth S, inventor. A method for sintering. C04B35/64. 2012.